Underneath ^10 Reduction
Clayworks Baltimore Md.

Kona F-4 Feldspar 2310
EPK 985
Dolomite 895
Whiting 189
Zircopax 381
Bentonite 95
Cobolt Carbonate 119
Chrome oxide 24