search  current discussion  categories  materials - frits 

a question about slip/frit

updated thu 30 may 02

 

Alisa Liskin Clausen on wed 29 may 02


Dear Susan,
The frit is like a bit of added "glue" to the clay slip because it adds
flux. Therefore the slip can hang on better to the clay beneathe it, giving
better adhesion and less likely to scale off.
regards from Alisa in Denmark