search  current discussion  categories  glazes - cone 8-10 

correction - underneath glaze cone10 red frrm clayworks baltiomre

updated sat 18 may 02

 

Judith Frederick on sat 18 may 02

Md

Sonya sent this to me

Underneath c10

NC-4 kona sodaspar 48.50
EPK 20.78
dolomite 18.80
whiting 3.97
tin oxide 7.95
rutile 2.40
I think this is the correct recipe. sorry for thr missinformation
earlier.
Judy in Baltimore