search  current discussion  categories  glazes - misc 

elca's liner glaze...

updated thu 23 may 02

 

Elca Branman on wed 22 may 02


I'm back from Guatemala, and almost normal.

Here is the liner glaze that I promised ..in response to James Bowen's
praises of same.. I am merely a conduit;never did anything except use it.

Betty's Satin White Cone 9-10 Red

Custer Spar.......5800
EPK ........2500
Dolomite.......1800
Whiting......300
Silica.....500

I like it slightly thin...
Elca Branman.. in Sarasota,Florida,USA
elcab1@juno.com