Paul on wed 22 may 02


does anyone have experience using ITC sprayed over bricks that have been
patched with greenpatch 421? I saw an old clayart post that mentioned this
may not be a good combination, but there was no response to it. My kiln
needs more patching than i can afford to use the itc patch with so i am
using greenpatch instead, and then i want to spray itc over it. Please let
me know if anyone has done this. thanks