search  current discussion  categories  kilns & firing - flues & venting 

exhaust manifold vs enamelling...

updated sun 16 jun 02

 

Philip Poburka on sat 15 jun 02


Right...'Enamelling' as such, is fun and not too difficult to do...
I have not done any in a long time now, but this inspires me to want to get
back to
it.

Potters posessing their own Kilns could certainly do it with but some
cursory introduction to the peramiters. It is such a cousin to Glazes in
it's way, only that the Glazes must 'fit' Iron, or what, rather than a Clay
Body.

Heating an enamelled Cast Iron Exhaust Manifold to 'clean' it, was another
matter!

That seemed too confused...unless one were to fire the Kiln only to the
temps just past where Carbon would burn off, which is way lower than
anyone's usual Fireing would tend to be...and why bother, when it could be
cleaned very well by other means?

Phil
el ve

----- Original Message -----
From: "Cindy Gatto"
To:
Sent: Friday, June 14, 2002 7:50 PM
Subject: Re: Exhaust Manifold


> Hi Ingeborg:
> We had a customer with an old cast iron bathtub
with
> cast iron feet that originally had ceramic coated feet on it. The feet
have
> since gotten all messed up and he wants to restore them. To make a long
story
> short, we fired them for him and the kiln was fine no problem at all. So
good
> luck in whatever you do.
> Sincerely:
> Cindy Gatto & Mark Petrin
> The Mudpit
> 228 Manhattan Ave
> Brooklyn NY 11206
> 718-218-9424
> mudpitnyc@aol.com
> www.mudpitnyc.com
>
>
____________________________________________________________________________
__
> Send postings to clayart@lsv.ceramics.org
>
> You may look at the archives for the list or change your subscription
> settings from http://www.ceramics.org/clayart/
>
> Moderator of the list is Mel Jacobson who may be reached at
melpots@pclink.com.