search  current discussion  categories  kilns & firing - misc 

inexpensive gas kiln - need some help

updated tue 25 jun 02

 

millenial_age on mon 24 jun 02


I am planning on building a 4 cu. ft gas fired kiln using four MR 750
venturi burners mounted vertically in an updraft design. I know
basically how I will construct it but it baffles me as to how to
create a good baffle and still get consistent heating results
throughout the kiln.

I am planning to have a 2' x 2' firing chamber surrounded by two
layers of ITC k-26 brick with a single layer vertically arranged flat
top much like the Minn. Flat Top.

Would someone have suggestions as to what kind of baffle to use with
vertically mounted burners?