Jim Tabor on thu 20 jun 02


Anyone with experience programing an LL kiln (Dynatrol controller) to
reach temp, cool some and then soak a few hours, cool some more and soak
again? I get an error 1 after it reaches the set temp of 2245. The
segments programed to soak at 1985 and 1925 did not function on the 2
firings attempted.

I would appreciate any suggestions to help program the kiln for a
successful crystal firing.

Thanks,

Jim Tabor