Alisa, all your recently posted glaze tests list this for the cool down:

>cool down max. per hour to 900c (1652f)

Do you mean to say a certain number of degrees per hour for the cool down?

Thanks for posting all the glaze tests! This is a huge amount of work.

Anne

Alisa Liskin Clausen on fri 14 jun 02


Dear Anne,
When I say cool down max. I figure that my kiln can cool down at the most
200c, so that is where I set it. But it cools a little slower than that.