June Perry on fri 28 jun 02
Here's is a Malcolm Davis Shino recipe. I don't know if this is the variation
(there are several out there) that you want.
Malcolm Davis Shino Cone 10, reduction
Nepheline Syenite 40.91 %
> Soda Ash 17.27
> Kona F-4 Soda Feldspar 9.82
> Edgar Plastic Kaolin 18.18
> Om #4 Kentucky Ball Clay 13.82
>
Regards,
June Perry
| |
|