warped tiles????????????

updated thu 4 jul 02

 

Miriam Steele on wed 3 jul 02


Have read a large number of posts on this problem but
have not seen the very obvious...at least ...to
me....solution.
When I make tiles, my slab roller is used, then
possibly, the rolling pin...lightly......they are
cut...lifted to a board...carefully.....then topped
with another board....on which I place a number of
things to LIGHTLY weigh it down evenly.
NO WARPAGE...GREAT TILES....did my kitchen area with
them... Don't understand everyone making this so
complicated. quoting some sort of %'s for curling on
this or that corner...Common sense will win out, every
time, folks.