Greg & Betsy Macdonald on sun 7 jul 02


----- Original Message -----=20
From: Greg & Betsy Macdonald=20
To: vandermeulen@NS.SYMPATICO.CA=20
Sent: Sunday, July 07, 2002 2:26 PM
Subject: Clay Dust


Get yourself a wet/dry workshop vacuum with a PLASTIC container body. =
Sears sells really powerful ones for about $100 +-. Open it up and using =
plastic plumbing fittings, retrofit the vacuum intake, into a tube that =
extends to about 3 inches from the bottom. Fill the container about half =
full with water and reassemble. If you vacuum frequently, any dust will =
end up in the water which you can empty into the flower garden =
periodically.

Good luck. Greg Macdonald