If it is any help to you I add paperclay (about 1/3) to my usual clay for small additions, this stopped all cracking of
small and thin pieces. I also Raku this combination with good results and very little if any cracks.

Try it and see. It would also work with terra-cotta clay.

Best wishes from Australia
Irene Poulton