search  current discussion  categories  safety - misc 

is there a food safe sealant?

updated sun 14 jul 02

 

claybair on sat 13 jul 02


I made a large pitcher drilled holes through it to attach a driftwood handle
with wire.
A customer wants it but also wants to use it to pour drinks. I didn't intend
it for food.
I told her I didn't think there was a food safe sealer but I'd research it.
It needs not only plug the holes but coat the wire as well.
I did offer to make her another one but she wants this one.
Any suggestions????

Gayle Bair - exhausted but had a great show today!
Bainbridge Island, WA
http://claybair.com