Leland G. Hall on wed 17 jul 02


Lately my favorite invention is my digital pyrometer. Raku has been going
much much better with it. Eyeballing glaze if fine, and still necessary,
but I sure am getting greater consistancy with the pyro. Some one the other
day was started a thread about these things (sorry, I don't remember who)
and I thought I'd mention that I got mine from OMEGA. A dual input, for
around eighty bucks. Love it. Easy to calibrate and had it over a year
with no problems. They have a great website with plenty of support too.
Hope this helps.

Leland Hall
Before The Wheel Enterprises
La Pine Oregon

Ann Brink on wed 17 jul 02


Hi Leland-I'm the one who wanted input on digital pyrometers. I went to the
Omega site and it's pretty confusing. Would you mind telling me the model #
or other distinguishing features of yours, so I can locate it on the
website? Thanks for writing.

Ann Brink in CA





> Lately my favorite invention is my digital pyrometer. Raku has been going
> much much better with it. Eyeballing glaze if fine, and still necessary,
> but I sure am getting greater consistancy with the pyro. Some one the
other
> day was started a thread about these things (sorry, I don't remember who)
> and I thought I'd mention that I got mine from OMEGA. A dual input, for
> around eighty bucks. Love it. Easy to calibrate and had it over a year
> with no problems. They have a great website with plenty of support too.
> Hope this helps.
>
> Leland Hall
> Before The Wheel Enterprises
> La Pine Oregon
>
>

Leland G. Hall on thu 18 jul 02


On Wed, 17 Jul 2002 08:11:28 -0700, Ann Brink wrote:

>Hi Leland-I'm the one who wanted input on digital pyrometers. I went to
the
>Omega site and it's pretty confusing. Would you mind telling me the model
#
>or other distinguishing features of yours, so I can locate it on the
>website? Thanks for writing.
>
>Ann Brink in CA
>
>
>
>
>
>> Lately my favorite invention is my digital pyrometer. Raku has been going
>> much much better with it. Eyeballing glaze if fine, and still necessary,
>> but I sure am getting greater consistancy with the pyro. Some one the
>other
>> day was started a thread about these things (sorry, I don't remember who)
>> and I thought I'd mention that I got mine from OMEGA. A dual input, for
>> around eighty bucks. Love it. Easy to calibrate and had it over a year
>> with no problems. They have a great website with plenty of support too.
>> Hope this helps.
>>
>> Leland Hall
>> Before The Wheel Enterprises
>> La Pine Oregon
>>
>>
>
>___________________________________________________________________________
___
>Send postings to clayart@lsv.ceramics.org
>
>You may look at the archives for the list or change your subscription
>settings from http://www.ceramics.org/clayart/
>
>Moderator of the list is Mel Jacobson who may be reached at
melpots@pclink.com.

Hi Ann. Yes, Omega's site is vast isn't it. Now that I think about it I
dug around in there a few days before I decided what I wanted. A couple of
points. I've never tried any one else's pyrometers, so I can't really
compare, except price wise, and features. Also, mine, which is a
model "HH12" dual input, is only good to 1999 degrees F., therefore, high
fire stoneware is out with this model. Furthermore, I already had a type K
thermocouple, which was good news since the two cheesy ones that came
standard
with this pyrometer were good only to about 600 F. I think I might try
calling them, asking for customer service, and explaining exatly what you
are trying to accomplish. I'd guess they can set you up with what you
need. But now that I think about how I wound up using my own thermlcouple,
maybe the competiveness of their pricing needs a second look. Good luck.
Leland Hall
Before The Wheel Enterprises

La Pine, Oregon