The Vessel Online on sat 20 jul 02


Steven I would suggest from the material I obtained from my local Smooth-on
rep. that you do not use a clay containing any iron in it as this will a)
decrease the life of your silicon and b)this may be why your silicon is not
hardening properly. I suggest going to the Smooth-on website for more info
and
and to find the rep. closest to your local.

Sincerely, Donald Burroughs