iandol on wed 24 jul 02
Dear Ababi,=20
Tom's original proposal was for a Cone Three Glaze based on the Unity =
abstract of a Cone 3 Bristol Glaze tested by A. S. Watt in 1916.
Anything which does not mature at that temperature will not get a tick =
based on Tom's original challenge.
Best regards,
Ivor
| |
|