search  current discussion  categories  kilns & firing - raku 

converiting a grill into a raku kiln...

updated thu 1 aug 02

 

Evan Clifford on tue 30 jul 02


I have a neighbor with a grill that they are trying to get rid of.
Would it be possible to convert the grill into a raku kiln? It is a
grill where the lid is on a hinge. Would a burner and ceramic fiber be
able to turn this grill into a kiln? Thanks.
-Evan

Tony Ferguson on wed 31 jul 02


Yup. and some ceramic button or steel fasteners to hold the fiber. Take a
look at my plans for converting a garbage can and an outdoor fire pit into a
raku kiln.

Tony

Thank you.

Tony Ferguson
Stoneware, Porcelain, Raku
www.aquariusartgallery.com
218-727-6339
315 N. Lake Ave
Apt 312
Duluth, MN 55806


----- Original Message -----
From: "Evan Clifford"
To:
Sent: Tuesday, July 30, 2002 2:15 PM
Subject: Converiting a grill into a raku kiln...


> I have a neighbor with a grill that they are trying to get rid of.
> Would it be possible to convert the grill into a raku kiln? It is a
> grill where the lid is on a hinge. Would a burner and ceramic fiber be
> able to turn this grill into a kiln? Thanks.
> -Evan
>
>
____________________________________________________________________________
__
> Send postings to clayart@lsv.ceramics.org
>
> You may look at the archives for the list or change your subscription
> settings from http://www.ceramics.org/clayart/
>
> Moderator of the list is Mel Jacobson who may be reached at
melpots@pclink.com.
>
>

Orchard Valley Ceramics Arts Guild on wed 31 jul 02


>I have a neighbor with a grill that they are trying to get rid of.
>Would it be possible to convert the grill into a raku kiln? It is a
>grill where the lid is on a hinge. Would a burner and ceramic fiber be
>able to turn this grill into a kiln? Thanks.
>-Evan

I don't see that you'd gain very much by starting with the BBQ.
Pretty much any container/vessel *could* be turned into a raku
kiln by lining it with ceramic fiber and adding a burner. But why
not just make a kiln with hardware cloth and fiber? There are good
step-by-step instructions in Steve Branfman's book.

(I have used old BBQs for sawdust firing and other low-temperature
firing processes. )