search  current discussion  categories  kilns & firing - raku 

ceramic buttons for raku building

updated thu 8 aug 02

 

ken kang on wed 7 aug 02


I use bolts and fender washers wraped with fiber for buttons, see =
pictures and instructions at:
http://photos.yahoo.com/rakuken2000
Look in gas kiln folder.

Aloha, Ken