BVCuma on fri 9 aug 02
Randy's red in the original unseen description=20
sounds like my glaze Jaded Bronze...
http://www.geocities.com/bvcuma/DSC00119.jpg
cept this one is a deep dark green
then into black. (raku)
This photo has not shown the true=20
reds and yellows of this work.
This was my sixth sculpture.. 1995
the first in the "venus" series=20
this was a multiple moulded piece...
Somewhat a shot in the dark..
this glaze was a great surprise.
just before I left Canada,
I used it two more times
with good consistancy in aesthetic response..
Gerstley based.