Ed Gould on wed 14 aug 02
THANKS EVERYONE FOR ALL YOUR RECOMMENDATIONS. I'LL TRY THEM ALL. Celia I would very much be interested in the formulae for New Rogers Black and Del Favero Luster. I regret that I do not have the skill to put photos on the net. I paid for a course not yet taken.
ed gould
columbia md
Marcia Selsor on wed 14 aug 02
Dear Ed
I think you can find these glazes online at Dewitt Giblet's site. He has a very extensive listing. I know the Del Favero Glaze is listed.
www.dinoclay.com/info/glazes/degraku.html
Marcia in Montana
Ed Gould wrote:
> THANKS EVERYONE FOR ALL YOUR RECOMMENDATIONS. I'LL TRY THEM ALL. Celia I would very much be interested in the formulae for New Rogers Black and Del Favero Luster. I regret that I do not have the skill to put photos on the net. I paid for a course not yet taken.
> ed gould
> columbia md
>
> ______________________________________________________________________________
> Send postings to clayart@lsv.ceramics.org
>
> You may look at the archives for the list or change your subscription
> settings from http://www.ceramics.org/clayart/
>
> Moderator of the list is Mel Jacobson who may be reached at melpots@pclink.com.
| |
|