insulating the outside of an electric kiln

updated tue 20 aug 02

 

terry sullivan on mon 19 aug 02


I've posted this before on this topic. Once again:

Linda Blossom added fiber insulation to the outside brick of her
electric kiln. Like Jonathan, you have to take the stainless jacket off,
wrap with the fiber, make the new holes, and add an extention to the
stainless when re covering the outside. I don't know if she's currently
on the list but Lisa Skeen is obviously in contact with her and perhaps
could get a full write up from Linda to post on Clayart.

Terry Sullivan
Nottingham Arts