search  current discussion  categories  techniques - stains 

: effects of oxides on stains and glazes

updated tue 27 aug 02

 

iandol on sun 25 aug 02


Dear Martin Howard,=20

I suggest you try to access a copy of:

Greg Daly, "Glazes and Glazing Techniques. A glaze journey" Kangaroo =
Press. 1995.

The illustrations will amaze you. I attended the summer school which =
provided the foundation work for this book. There were 28 students. By =
the end of the third day we had produced over 10,000 effects from seven =
base glazes fired to cone 10.

Best regards,

Ivor Lewis.