RPeckham@COOKSONELECTRONICS.COM on thu 5 sep 02


My last studio was wall to wall carpet. My next one won't be. What I did
was buy a 6 hp wet/dry Ridgid vacuum. I originally bought it for digging
post holes, works wonderfully. In the studio I would occasionall cover
the floor with water, and vacuum it up. No dust, voila!

I imagine it would work as well on a rough concrete floor. Just cover it
with water, and brush it with a push broom, then vacuum up the water.

You may even be able to glaze a pot with the sludge.