search  current discussion  categories  materials - misc 

water warden and waxing

updated fri 6 sep 02

 

Carole Fox on thu 5 sep 02


Okay- I got the stuff and sprayed it on my white, terra sigillata =
covered pots, put 'em by the window and wahoo!- there was no trace of it =
on the surface of the pot. I have been waxing my pots up to now and was =
wondering if you can still wax if you are using water warden. If so, =
when to wax?- before or after the water warden treatment?

Also- I was initially thinking that this product would make my porous =
raku clay able to hold water. However, I now get the impression that =
this product is more for earthenware (protection from weathering). I =
would appreciate hearing from others who have used this product.
Thanks-
Carole Fox
Elkton, MD
cfox@dca.net