> I am looking for something that will give the deep blue look of
> Cobalt Oxide and Cobalt Carbonate but have yet to find anything
> cheaper.
>
> Does anyone know of an alternative to the very expensive cobalt
> materials or a place to get them at a cheap price?
>
> I recently made:
>
> Ball Clay 50%
> Kaolin 50%
>
> Add:
> Cobalt oxide 4%
> Cobalt Carbonate 7%
>
> And while the blue is great!!!!! it is an expensive formula. I apply
> it to wet greenware and then use a clear glossy glaze over it.
>
>
____________________________________________________________________________
__
> Send postings to clayart@lsv.ceramics.org
>
> You may look at the archives for the list or change your subscription
> settings from http://www.ceramics.org/clayart/
>
> Moderator of the list is Mel Jacobson who may be reached at
melpots@pclink.com.