Craig Clark on wed 18 sep 02
Evan, no you don't need a pug mill to mix up a clay body........they're
just a whole lot-a-help. All you really need is an appropriate sized
container of some type (a kiddie pool works well, the hard plastic kind),
the components of the body that you want to mix, water, your feet and some
friends who might enjoy an evenining of faux "grape stomping" and the
associated swillling of beverages of choice (you can do it on your own it's
just a hoot with a buncha folks.)
Craig Dunn Clark
619 East 11 1/2 st
Houston, Texas 77008
(713)861-2083
mudman@hal-pc.org
----- Original Message -----
From: "Evan Clifford"
To:
Sent: Wednesday, September 18, 2002 4:29 PM
> Can a claybody be mixed like a glaze or must a pugmill be used...
> Thanks in advance.
>
> -Evan
>
>
____________________________________________________________________________
__
> Send postings to clayart@lsv.ceramics.org
>
> You may look at the archives for the list or change your subscription
> settings from http://www.ceramics.org/clayart/
>
> Moderator of the list is Mel Jacobson who may be reached at
melpots@pclink.com.
| |
|