search  current discussion  categories  techniques - spraying 

mouth operated sprayers for glaze - another type

updated thu 19 sep 02

 

Kurt Wild on wed 18 sep 02


At 12:19 PM 9/17/02 -0400, John Hesselberth wrote:
>I need some help. I want to find a small spray gun that I can use to
>apply accents of several glazes. I would like to have several glazes
>available without the trouble of changing over one of the more standard
>air-compressor-operated guns to another glaze every few seconds. .......
>.......Question 2: Does anyone know of other sources/brands for sprayers .....

Here is the URL of a site where you can see, read about and purchase a
super small sprayer that I have used and recommend highly!
http://www.x-actoblades.com/preval/preval.htm


From my favorite chair - leg elevated, now in a short "walking" cast,
slowly getting better - laptop on my lap - phone at my side 715-425-5715
Kurt

Dwiggins, Sandra (NCI) on wed 18 sep 02


Kurt...
Thanks for the tip. This looks great!
Sandy

> -----Original Message-----
> From: Kurt Wild [mailto:kurtwild@ATTBI.COM]
> Sent: Wednesday, September 18, 2002 3:57 PM
> To: CLAYART@LSV.CERAMICS.ORG
> Subject: Re: Mouth operated sprayers for glaze - another type
>
>
> At 12:19 PM 9/17/02 -0400, John Hesselberth wrote:
> >I need some help. I want to find a small spray gun that I can use to
> >apply accents of several glazes. I would like to have several glazes
> >available without the trouble of changing over one of the
> more standard
> >air-compressor-operated guns to another glaze every few
> seconds. .......
> >.......Question 2: Does anyone know of other sources/brands
> for sprayers .....
>
> Here is the URL of a site where you can see, read about and purchase a
> super small sprayer that I have used and recommend highly!
> http://www.x-actoblades.com/preval/preval.htm
>
>
> From my favorite chair - leg elevated, now in a short "walking" cast,
> slowly getting better - laptop on my lap - phone at my side
> 715-425-5715
> Kurt
>
> ______________________________________________________________
> ________________
> Send postings to clayart@lsv.ceramics.org
>
> You may look at the archives for the list or change your subscription
> settings from http://www.ceramics.org/clayart/
>
> Moderator of the list is Mel Jacobson who may be reached at