Hank Murrow on wed 18 sep 02


>Hi Hank:
>I carried an article about your shino glazes around with me for
>ages, until I found the low melt spodumene at Georgies. Then my
>kiln was delivered. Then I lost the magazine..which one was it and
>is there a place...Clayart?...that I can get the shino recipes
>again? I've been thru all my CM back issues and I'm afraid I lost
>the copy.
>I'd be ever so grateful. I can still see those gorgeous glazes.
>The shinos I've used don't look quite so lucious.

Thanks, Susan Antinori



Dear Susan;

If you check this site
(http://www.ceramicsmonthly.org/mustreads/shinofire.asp) you will
find the articles. Good luck in your work!

Cheers, Hank in Eugene

Also in French (http://perso.wanadoo.fr/smart2000/shinos.htm) with the pics.