search  current discussion  categories  techniques - slips 

cleaning slip trailers

updated fri 20 sep 02

 

Stephen Parry-Thomas on thu 19 sep 02


Hi folks,

Somebody sent me an email off line asking me how we clean our slip trailers.
Sorry I've deleted your email. So I've put it on here in the hope you will
see it. This is what we do, just add several small stones inside your trailer
add water, put Motorhead on the CD player and shake in time to the music, a
few seconds later the trailer will be clean inside. Keep the stones for
later. Our slip trailers are large plastic bottles they hold about half a
litre (just over a pint). When you have 50 trailers to clean that the
quickest, unless you know another way?

Steve


Stephen & Karen Parry-Thomas
http://www.morrigancraftpottery.co.uk
steve@morrigancraftpottery.co.uk