Carol Tripp on thu 19 sep 02
Charles wrote,
>In case Ron and John are busy, let me supply one answer to your "creamy
>white liner glaze" ^6:
>
>Try Tony Hansen's 5 X 20 with 10% Zircopax. It produces a sort of antique
>white.
I have used Tony's 5x20 with Zircopax. In my experience, it okay only on
it's own but it will crawl if you layer it with anything else. In fact, I
had a problem with it occasionally crawling all on it's own. Your
experience may vary.
Best regards,
Carol