Harold Miller on sat 21 sep 02


I'm looking for a source in the Austin-San Antonio, Texas,
region of new or used 2300=BA-2400=BA hard arch #2 & #3
firebrick.

Lily Krakowski on tue 15 oct 02


Cheryl's query about firing temp of old kilns makes me wonder. Is there a
way of testing soft brick for its firing temp? Besides trying to overfire
it? I know hard brick often/generally ? comes stamped with I.D...but soft
brick?