search  current discussion  categories  people 

warren mackenzie pot on ebay

updated sun 22 sep 02

 

David Dahlquist on sat 21 sep 02


Item # 2055084682. I was tempted to make a bid, but then I re-read the =
description to find it had been cracked, then to see that the potter =
glued it together? Doesnt sound right to me. Especially from this =
potter. Or am I crazy? Does this sound right? I thought pots like this =
where pitched.
"There is a thin flake which is difficult to see on the inside bottom =
edge of the cover approximately 1/4 inch by 1/2 inch, which when we =
bought the pot. The cover was dropped by Warren when we purchased the =
pot. He took it into the house, glued it in place and handed it to us =
saying "good as new" He did not offer to reduce the price and we did not =
ask him to do so. Absolutely nothing else, no other damage, flawless =
inside and out. "
dave