Glaze addicts,
When you test either the white glaze suggested by Mel Jacobson or Chris
Stanley's offering, be aware both these glazes are relatively low in
expansion. While they will likely fit porcelain, they may shiver from
stoneware clay bodies. I looked at both recipes with Insight to arrive at
this conclusion.
Dave Finkelnburg, watching fall arrive in Idaho
| |
|