search  current discussion  categories  wheels - manufacturers 

shimpo rk2 ring results

updated tue 24 sep 02

 

Jon Faber on mon 23 sep 02


got a new belt.
(thanks for the specs Phil)

put the cone ring back on
(thanks for the tip Earl)

Wheel definately performs better but still hangs up
when centering dry. I think this just may be the
nature of the beast.

Even the brent C's that i am used to struggle a bit at
the same point.

I have to check the archives again to see what me and
vince and other have recommended for similar troubles.

I have to say, even with these troubles, I am
absolutely amazed at the simplicity of this machine.

I agree that putting the motor on the pedal mount was
simply a bad idea but I can not get over the
simplicity of it all.

Thanks again for the help.
I imagine this would have have been much more
difficult without the list.

jon