search  current discussion  categories  kilns & firing - raku 

raku thanks!

updated tue 1 oct 02

 

Ababi on mon 30 sep 02


I want to thank all of you, the people that helped me to solve my raku kiln problems.
The shelf was too big
The hole in the top was too wide
The hole were the fire enters into the kiln was plugged with dirt
The pressure of the gas was too low.
After solving these problems I realized that:
After the firing my heart was beating like a machine gun!
I hardly sell any of these works,( "the glazes is cracked").

So I stick to ^6

I might use that kiln for saggar.

I shall use my knowledge to assist anyone who needs.
I shall keep the page of new raku and I keep on a CD the information I got from the net
means from you.(For you!)

Ababi Sharon
Glaze addict
Kibbutz Shoval Israel
ababisha@shoval.org.il
http://members4.clubphoto.com/ababi306910/