c10 clear glaze

updated sat 5 oct 02

 

June Perry on fri 4 oct 02


The Imsil-A25 is Amorphous silica, a fine form of silica, which can help to
lessen glaze crazing.

Regards,
June

Charles Moore on fri 4 oct 02


June,

I have a ^6 glaze that I like a great deal, but which show a fine crazing
used alone or on top of other glazes.

Where do you get Imsil-A25, Amorphous silica? To prevent crazing, do you
use the Imsil-A25 in place of all the silica? Or do you add it in
increments?

Thanks,

Charles
Sacramento

----- Original Message -----
From: "June Perry"
To:
Sent: Friday, October 04, 2002 6:39 AM
Subject: C10 Clear glaze


> The Imsil-A25 is Amorphous silica, a fine form of silica, which can help
to
> lessen glaze crazing.
>
> Regards,
> June
>
>
____________________________________________________________________________
__
> Send postings to clayart@lsv.ceramics.org
>
> You may look at the archives for the list or change your subscription
> settings from http://www.ceramics.org/clayart/
>
> Moderator of the list is Mel Jacobson who may be reached at
melpots@pclink.com.