search  current discussion  categories  glazes - misc 

clay to match glaze

updated fri 18 oct 02

 

Ilene Richardson on tue 15 oct 02


Here is a true beginners question:
If I begin by using ready made glazes, (because I need to practice
firing and such on my new kiln) and use
Duncan Concepts Glazes,
Underglazes with Duncan Envisions Clear Glaze,...
These fire at 06 on a clay that is fired Bisque 04, then please tell me
which Clay, to fire at 04, would be a good match for handbuilding and
throwing.

I was looking at Standard clays or Laguna which seem easy to order online.

Whew! That was a lot to organize for this question that I finally got
the nerve to ask.
Ilene

Ilene Richardson on thu 17 oct 02


Whoops, I had it backwards.... :-
The glaze it listed incorrectly on the website, that is why I had it
confused, besides as being new to this once again I'm already confused.

Ilene


[Duncan Concepts Underglaze]
[BigCeramicStore Home]

[Home] [Product Index]
[Help?]
[Articles / Links]
[FAQ]


The first coat is translucent. The second is semi-opaque. Three coats
give bisque full coverage. All are non-toxic. Can be used without
clear glaze, but is designed for use with Envision

Clear glaze or Diamond Clear (brush-on or dipping). Fire to cone 06 on
bisque 04.