crystalin glaze

updated fri 18 oct 02

 

myersw on thu 17 oct 02


Fellow Potters:
Is it possible to make a glaze with large crystals at cone 6 ox.? If =
so, does anyone have a recipe for it? Thanks to any kind person that =
replys.

Wallace=20

Brooks Ratledge on thu 17 oct 02


yes - there are one or two recipes in Bailey's Glazes, Cone 6 and I think
Fara Shimbo's book has several cone 6 macrocrystalline glazes. Patricia
Harden
-----------------------------------------------------
Click here for Free Video!!
http://www.gohip.com/free_video/

-----Original Message-----
From: myersw
To: CLAYART@LSV.CERAMICS.ORG
Date: Thursday, October 17, 2002 11:47 AM
Subject: crystalin glaze


Fellow Potters:
Is it possible to make a glaze with large crystals at cone 6 ox.? If so,
does anyone have a recipe for it? Thanks to any kind person that replys.

Wallace

____________________________________________________________________________
__
Send postings to clayart@lsv.ceramics.org

You may look at the archives for the list or change your subscription
settings from http://www.ceramics.org/clayart/

Moderator of the list is Mel Jacobson who may be reached at
melpots@pclink.com.