search  current discussion  categories  materials - rutile 

was: rutile blues -- now reduction differences inside and out?

updated thu 31 oct 02

 

Connie Woodward on wed 30 oct 02


I've notice while firing rutile blue stuff and shinos, that often a mug or
vase or jar will turn out beautiful on the inside and ugly
biege/white/grey on the outside.

Are there differences in the amount of reduction on the inside of vessels
then the outside? or would the difference only be to the glaze thickness?

thanks,

Connie


--
=================================================
Connie Woodward Karattopp Pottery 713-256-5907
Navasota, TX www.karattopp.com connie@karattopp.com