Jim Larkin on thu 31 oct 02
Alycia
Bryant Refractories in Tulsa will have any kind of refractory you might =
want. Their number is 1-800-463-1162.=20
Jim
Jim Larkin
Fox Pass Pottery
379 Fox Pass
Hot Springs, Arkansas
71901
foxpass@aristotle.net
>Hello All
I live and pot in central Oklahoma and I am wanting to build my very own =
gas fired brick kiln.
Do you all have any suggestions on where to buy fire bricks and what =
brand of bricks are best. I would be willing to travel. (have truck have =
trailer) It seems there is non where around this area that sells the =
right kinds of bricks.
Thank you very much
Alycia in Edmond Oklahoma.<
| |
|