search  current discussion  categories  kilns & firing - misc 

over fire

updated fri 1 nov 02

 

Ababi on thu 31 oct 02


Hello Clayart!
I did not plan properly the control of my kiln. Therefore I believe I had 2-3 hours soaking
in 1220C mainly ^6.
I have some questions.
If the works, tests, will survive. Will they still be ^6?
I prepared bars for absorption tests. Again, are they still ^6?
Thanks Ababi.

When I test new glazes I see the horizon, I see I get the best glazes ever.
When I reach the horizon, I find another hill, another idea to test.
Ababi Sharon
Glaze addict
Kibbutz Shoval Israel
ababisha@shoval.org.il
http://members4.clubphoto.com/ababi306910/
http://www.milkywayceramics.com/cgallery/asharon.htm