Ron Collins on sat 2 nov 02


For those of you, who might not know, if you want to roll a perfect =
stopper...remember, it follows an arc...so when you "roll it" make a =
carrot, and let it roll in the circle that it wants to do....you will =
end up with a stopper, not a coil, and it will fit-read Tommy =
Humphries's post-on setting the stopper....learning to make stoppers is =
a handy thing to know....Melinda Collins, Antigua, Guatemala