search  current discussion  categories  glazes - cone 4-7 

^6 reduction - dan hill

updated sat 9 nov 02

 

Eric Suchman on thu 7 nov 02


Dan,
Boron....in the form of borax?
Eric in Oceanside

> From: June Perry
> Reply-To: Ceramic Arts Discussion List
> Date: Thu, 7 Nov 2002 07:57:07 EST
> To: CLAYART@LSV.CERAMICS.ORG
> Subject: Re: ^6 reduction - Dan Hill
>
> Dan,
>
> Are you using soda ash for your C6 soda firings, or do you mix some boron in
> with the mix?
> I did a couple of C10 firings before I moved and now that I'm mostly doing C6
> oxidation, I'd like to stay with the C6 clay and try it in my mini
> soda/wood/diesel kiln.
> Would love some feedback on your process.
>
> Regards,
> June Perry
> http://www.angelfire.com/art2/shambhalapottery/index.html
>
> ______________________________________________________________________________
> Send postings to clayart@lsv.ceramics.org
>
> You may look at the archives for the list or change your subscription
> settings from http://www.ceramics.org/clayart/
>
> Moderator of the list is Mel Jacobson who may be reached at
> melpots@pclink.com.

June Perry on thu 7 nov 02


Dan,

Are you using soda ash for your C6 soda firings, or do you mix some boron in
with the mix?
I did a couple of C10 firings before I moved and now that I'm mostly doing C6
oxidation, I'd like to stay with the C6 clay and try it in my mini
soda/wood/diesel kiln.
Would love some feedback on your process.

Regards,
June Perry