Alisa Liskin Clausen on thu 7 nov 02


Besides the glazes mentioned, Chris Wolffe's Plum, also in the archives, is
a warm brown with some speckling. Glossy and goes very well under either
his Cream Glaze, in archives, or the Cream of Mushroom you have already.
However, can become very blue opalescent as well where they are layered.