search  current discussion  categories  glazes - cone 4-7 

satin matt c6 ox

updated tue 12 nov 02

 

Tom Buck on mon 11 nov 02


Caroline Austin of UK seeks recipes for satin matt C6 oxidation. I urge
her to find two books: Michael Bailey (Bath, UK) wrote "Cone 6 Glazes" and
has many recipes that could serve. North Americans John Hesselberth & Ron
Roy wrote
"Mastering Cone 6 Glazes" (self-published) and it also has some C6 matt
glaze recipes. Both these new books are superb and offer great help to
potters firing to Cone 6 in electric kilns.
peace. Tom B.

Tom Buck ) -- primary address.
"alias" or secondary address.
tel: 905-389-2339 (westend Lake Ontario, province of Ontario, Canada).
mailing address: 373 East 43rd Street, Hamilton ON L8T 3E1 Canada