Dwiggins, Sandra (NIH/NCI) on tue 12 nov 02
Ron and all others who know this clay....
Can I use this for a woodfire??? I can use Standard's Grolleg, but my
supplier was out, so I bought this instead....did I make a mistake?
TIA,
Sandy
Ron Roy on wed 13 nov 02
Hi Sandy,
It is vitrfied (0.0 absorbency at cone 10) - if you are firing above that -
well - expect some warping with some forms - probably better to keep it out
of direct flame.
Some like some heat induced adjustments to form - and I do with some forms
- just a matter of finding the right way to get it.
RR
>Ron and all others who know this clay....
>Can I use this for a woodfire??? I can use Standard's Grolleg, but my
>supplier was out, so I bought this instead....did I make a mistake?
>TIA,
>Sandy
Ron Roy
RR#4
15084 Little Lake Road
Brighton, Ontario
Canada
K0K 1H0
Phone: 613-475-9544
Fax: 613-475-3513
| |
|