Kat Valenzuela on thu 14 nov 02


Hey All:
Let me properly introduce myself. I work with Tony Hansen at Plainsman Clays.
Yah! That should be sufficient..
Ok, Tony always tells me that the glazes he published are starting points.
Since everyone uses different clays with various methods. The most
important part is knowing how to alter your recipe when it is not doing
what you want.
That is why he created insight.
So in his defence, the recipes are not intended to fit everybody's clay
bodies.
Crummy - I wish there was one solution one answer.

Yet one thing I find odd, is that the recipe fits on porcelain and not on
stoneware. Usually the opposite is more likely.

Kat in the Hat