correction: glaze test for crawl glaze 1, cone 6-9, ox.

updated mon 18 nov 02

 

Alisa Liskin Clausen on sun 17 nov 02


RIGHT! good you caught that.

Should read 21 Magnesium Carbonate,
not Manganese.

>Recipe:
>
>21 Manganese Carb.
>57 Neph. Syenite
>22 Ball Clay