Chris, I think Jim Brasheer byes his b-mix dry blended in the bag. His
students get to learn how to mix clay, play with reclaim, but he gets b-mix.
I think hes in fairbanks, chat chat chat. For what you pay to ship water
you can buy a mixer and you'll always know where the chunks are coming from.
If you havent thrown the stuff fluffy out of th emixer instead of those
super pugmills you gotta try it out.

S






>From: Kris Bliss
>Reply-To: Ceramic Arts Discussion List
>To: CLAYART@LSV.CERAMICS.ORG
>Subject: Re: what is it with laguna?
>Date: Mon, 11 Nov 2002 15:09:01 -0900
>MIME-Version: 1.0
>X-Originating-IP: [66.58.157.248]
>Received: from mc4-f3.law16.hotmail.com ([65.54.237.138]) by
>mc4-s14.law16.hotmail.com with Microsoft SMTPSVC(5.0.2195.5600); Mon, 11
>Nov 2002 18:14:28 -0800
>Received: from mercury.acers ([209.115.31.35]) by mc4-f3.law16.hotmail.com
>with Microsoft SMTPSVC(5.0.2195.5600); Mon, 11 Nov 2002 18:14:28 -0800
>Received: from LSV (209.115.31.36) by mercury.acers (Worldmail 1.3.167); 11
>Nov 2002 21:14:15 -0500
>Received: from LSV.CERAMICS.ORG by LSV.CERAMICS.ORG (LISTSERV-TCP/IP
>release 1.8d) with spool id 225126 for CLAYART@LSV.CERAMICS.ORG;
>Mon, 11 Nov 2002 21:13:56 -0500
>Received: from 64.4.15.107 by LSV.CERAMICS.ORG (SMTPL release 1.0d) with
>TCP; Mon, 11 Nov 2002 19:08:43 -0400
>Received: from mail pickup service by hotmail.com with Microsoft SMTPSVC;
>Mon, 11 Nov 2002 16:09:01 -0800
>Received: from 66.58.157.248 by lw10fd.law10.hotmail.msn.com with HTTP;
>Tue, 12 Nov 2002 00:09:01 GMT
>Approved-By: melpots2@PCLINK.COM
>X-OriginalArrivalTime: 12 Nov 2002 00:09:01.0566 (UTC)
> FILETIME=[B45029E0:01C289DF]
>Message-ID:
>Sender: Ceramic Arts Discussion List
>Comments: To: jpacini@lagunaclay.com
>Return-Path: owner-clayart@LSV.CERAMICS.ORG
>
>Dear Jon and all,
>thank you for waiting for my reply, things have been lets say, busy.
>here is my story.
>last summer i had clay art tacoma order some b-mix for me mixed firm. i
>recieved 800 # of it.. batch #31053. when it arrived i tried throwing it,
>it
>felt like a clay i made in school with to much v gum.. Is this me? I had
>jen
>try some, same..she said it felt "puffy"..Ian pronounced it un throwable.
>then we opened a box in the center of the load. full of chunks hard nasty
>seemed like unmixed something.. ok day of stomping . then i called clay art
>and didn't get the guys name (not joe) his response was awwww. i left a
>coupla messages for joe but. so i figure i'm stuck. (again, alaska is too
>far away to return this much stuff). I call clay art again and tell them i
>do not want them to send me the rest of the batch (as planned) and get some
>regular b mix. it seemed ok and then we get down to the last oh 600# and
>chunks start turning up..ian throws the whole mess into the pug mill, i
>have
>just recieved 2 tons of new batch and wonder am i stuck again???
> write a rant to clayart, thanks guys, call clay art tacoma and insist on
>talking to Joe (takes two days to get to him).
> Joe says document, save chunks, call laguna. o.k. meantime, jon at
>laguna sees my rant and sends e-mail, see below.
> So i am thawing out a box of the first firm nasty stuff to send jon a
>few
>#s of the stuff.
> and will send him copies of the invoice. ( i don't have a fax)
> the second order we had trouble with, OH MY GAWWD! it's the same batch,
>those people at clay art sent me the rest of the bad batch. no wonder we
>haven't had any decent clay!! we have been using recyle from be for the bad
>stuff..
>
> we now i have 2 ton of as near as i can tell, 5 or 6 batchs, so there
>has
>got to be some decent clay in there.
> So the saga continues.....i'll keep you guys posted
>thanks for listening, and your moral support.
>
>keep centered, and may the forms be with you.
>kris in alaska
>where there is STILL no snow.
>
>
>>From: "Jon Pacini"
>>
>>Hi Kris---Saw your posting on Clayart and wanted to touch base with you.
>>Can
>>you please contact me directly? jpacini@lagunaclay.com If you can send me
>>batch #s I would like to see when and by whom that particular clay was
>>made
>>so I can rectify this problem. The batch #s are 5 digits hand stamped on
>>the
>>sides/ top of the boxes. Could you possibly forward a box/pug of the clay
>>to
>>me?? I would like to see how prevalent the contamination is and if I can
>>identify the material.
>> Could you also forward copies of your receipts from Clay Art Center
>>by
>>Fax?
>>
>>Thanks
>>
>>Jon Pacini
>>Clay Manager
>>Laguna Clay Co
>>
>
>
>_________________________________________________________________
>Tired of spam? Get advanced junk mail protection with MSN 8.
>http://join.msn.com/?page=features/junkmail
>
>______________________________________________________________________________
>Send postings to clayart@lsv.ceramics.org
>
>You may look at the archives for the list or change your subscription
>settings from http://www.ceramics.org/clayart/
>
>Moderator of the list is Mel Jacobson who may be reached at
>melpots@pclink.com.


_________________________________________________________________
STOP MORE SPAM with the new MSN 8 and get 2 months FREE*
http://join.msn.com/?page=features/junkmail